Home>ISO Standards>BS ISO 10471:2018 pdf free

BS ISO 10471:2018 pdf free

BS ISO 10471:2018 pdf free.Glass-reinforced thermosetting plastics (GRP) pipes
The method allows the use of either bearing plates or beam bars for loading the test piece, subject to reporting the choice used. Either method may be used for measurements of relative vertical deflection up to 28 %. When it is expected that 28 % deflection is going to be exceeded then the procedure is limited to the use of at least one beam bar.
The surfaces shall be provided by a pair of bearing plates, in accordance with 5.2.2, or a pair of beam bars, in accordance with 5.2.3, or a combination of one such plate and one such bar. However, if the applied force is expected to cause a relative deflection in excess of 28 %, at least one of the surfaces shall be a beam bar. The surface’s major axes shall be perpendicular to and centred on the direction of application of force F by the compressive loading machine, as shown in Figure 1. The surfaces to be in contact with the test piece shall be flat, smooth, clean and parallel.
The plate(S) shall have a width of at least 100 mm and a length at least equal to the length of the test piece (see Clause 6). They shall be sufficiently stiff so that they do not visibly bend or otherwise deform during the test.
Each beam bar shall be sufficiently stiff that it does not visibly bend or otherwise deform during the test. Each beam bar shall have a length at least equal to the length of the test piece (see Clause 6) and a flat face (see Figure 1) without sharp edges. The width of the flat face shall be 15 mm to 55 mm.
The beam bars shall be constructed and supported so that no other surface of the beam bar structure comes into contact with the test piece during the test.BS ISO 10471 pdf download.

Related standards